High corrosion resistance:
With Fe materials and light metals depending on the selected conversion coating, at least 240 h without sub-surface migration / infiltration into the scratch track in accordance with DIN EN ISO 9227 NSS.
Temperature stability:
Range up to 400°C
Normal Annealing Temperature:
120°C ºC – 180 ºC
Normal Layer Thickness:
from 40 µm to 300 µm
Color:
All colors and gloss qualities can be represented
Resistance to:
Complies with the EU Scrap Vehicle Directive:
With Fe materials and light metals depending on the selected conversion coating, at least 240 h without sub-surface migration / infiltration into the scratch track in accordance with DIN EN ISO 9227 NSS.
Temperature stability:
Range up to 400°C
Normal Annealing Temperature:
120°C ºC – 180 ºC
Normal Layer Thickness:
from 40 µm to 300 µm
Color:
All colors and gloss qualities can be represented
Resistance to:
- UV radiation (sunlight)
- Fuels, brake fluids, oils, conventional solvents
- Biodiesel
- Acids > pH 4 in the case of epoxy powder
- Alkali < pH 9 in the case of epoxy powder
- Stone impact resistance
Complies with the EU Scrap Vehicle Directive:
- Lead: absent
- Chromium 6+: absent
- Cadmium: absent
- Mercury: absent